Multi wall carbon nanotube (MWCNT) doped ZnO nanofibers were fabricated by electrospinning for the first time. We have successfully demonstrated the photocatalytic activity of doped nanofibers under visible light. Scanning electron microscopy showed that the diameter of MWCNT-doped ZnO nanofibers varied from 120 to 300 nm without agglomeration of MWCNT. Fourier transform infrared spectroscopy and X-ray diffraction studies proved the formation of ZnO bond and wurtzite structure with smaller crystal size in doped nanofibers. Raman spectra demonstrated slight shift in bond position after nanofiber doping, indicating the chemical bond between MWCNT and ZnO. X-ray photoelectron spectroscopy showed that ZnOC bond were formed in the nanofibers and the energy band gaps were 3.11 and 2.94 eV for pure and doped ZnO nanofibers, respectively. Thermal gravimetric analysis revealed a total weight loss of 55% with no variation in mass reduction at temperature above 460°C. In comparison with ZnO nanofibers, a 7-fold enhancement in photocatalytic activity was observed under UV light as a result of delaying electron-hole recombination as verified by photoluminescence spectroscopy. The improvement in the visible light photocatalytic performance was assigned to the role of MWCNT as photosensitizer and the synergistic effect between MWCNT and ZnO.

Visible light photocatalytic activity of novel MWCNT-doped ZnO electrospun nanofibers

ZANETTI, Marco;
2012-01-01

Abstract

Multi wall carbon nanotube (MWCNT) doped ZnO nanofibers were fabricated by electrospinning for the first time. We have successfully demonstrated the photocatalytic activity of doped nanofibers under visible light. Scanning electron microscopy showed that the diameter of MWCNT-doped ZnO nanofibers varied from 120 to 300 nm without agglomeration of MWCNT. Fourier transform infrared spectroscopy and X-ray diffraction studies proved the formation of ZnO bond and wurtzite structure with smaller crystal size in doped nanofibers. Raman spectra demonstrated slight shift in bond position after nanofiber doping, indicating the chemical bond between MWCNT and ZnO. X-ray photoelectron spectroscopy showed that ZnOC bond were formed in the nanofibers and the energy band gaps were 3.11 and 2.94 eV for pure and doped ZnO nanofibers, respectively. Thermal gravimetric analysis revealed a total weight loss of 55% with no variation in mass reduction at temperature above 460°C. In comparison with ZnO nanofibers, a 7-fold enhancement in photocatalytic activity was observed under UV light as a result of delaying electron-hole recombination as verified by photoluminescence spectroscopy. The improvement in the visible light photocatalytic performance was assigned to the role of MWCNT as photosensitizer and the synergistic effect between MWCNT and ZnO.
2012
359
42
48
http://www.sciencedirect.com/science/article/pii/S1381116912000970
Morasae Samadi; Hossein Asghari Shivaee; Marco Zanetti; Ali Pourjavadi; Alireza Moshfegh
File in questo prodotto:
File Dimensione Formato  
Morasa Journal of Molecular Catalysis A Chemical.pdf

Accesso riservato

Tipo di file: PDF EDITORIALE
Dimensione 1.43 MB
Formato Adobe PDF
1.43 MB Adobe PDF   Visualizza/Apri   Richiedi una copia
2012- Postprint - Zanetti Samadi- OA 24m.pdf

Open Access dal 29/03/2014

Tipo di file: POSTPRINT (VERSIONE FINALE DELL’AUTORE)
Dimensione 1.74 MB
Formato Adobe PDF
1.74 MB Adobe PDF Visualizza/Apri

I documenti in IRIS sono protetti da copyright e tutti i diritti sono riservati, salvo diversa indicazione.

Utilizza questo identificativo per citare o creare un link a questo documento: https://hdl.handle.net/2318/102296
Citazioni
  • ???jsp.display-item.citation.pmc??? ND
  • Scopus 194
  • ???jsp.display-item.citation.isi??? 166
social impact