We report the synthesis and surface functionalization of MCM-41-like mesoporous silica nanoparticles (MSNs) with spheroidal shape and particle size of 141 +- 41 nm. The success of surface functionalization with aminopropyl and sodium ethylcarboxylate groups (giving amino-MSN and carboxy-MSN, respectively) was ascertained by infrared spectroscopy and z potential measurements. The former showed the decrease of surface silanol groups and the corresponding appearance of signals related to NH2 bending mode (dNH2) at 1595 cm-1 and COO- stretching (nas and nsym) at 1562 and 1418 cm-1. The latter showed a change in surface charge, in that the isoelectric point (IEP) changed from pH 3–4.5 to 8.5 when the MSN was functionalized with the amino groups, while carboxy-MSN showed a more negative charge in the whole pH range with respect to MSN. The hydrophilic character of the prepared materials was ascertained by quantitative microgravimetric measurements, allowing the calculation of the average isosteric adsorption heat (qst). This was found to be 51 +- 3 kJmol-1, 61+- 4, and 65 +- 3 kJmol-1 for MSN, amino- MSN, and carboxy-MSN samples, respectively. The increase in qst after functionalization can be ascribed to the specific interaction of water molecules with the functionalizing agents, in agreement with a higher basicity with respect to silanol groups. Moreover, the possibility of multiple H-bonding interactions of water molecules with the carboxylate anion is put forward to account for the higher water uptake with respect to parent MSN.
Influence of surface functionalization on the hydrophilic character of mesoporous silica nanoparticles
BOTTINELLI, EMANUELA DIANA;CELI, Luisella Roberta;MAGNACCA, Giuliana;BERLIER, Gloria
2015-01-01
Abstract
We report the synthesis and surface functionalization of MCM-41-like mesoporous silica nanoparticles (MSNs) with spheroidal shape and particle size of 141 +- 41 nm. The success of surface functionalization with aminopropyl and sodium ethylcarboxylate groups (giving amino-MSN and carboxy-MSN, respectively) was ascertained by infrared spectroscopy and z potential measurements. The former showed the decrease of surface silanol groups and the corresponding appearance of signals related to NH2 bending mode (dNH2) at 1595 cm-1 and COO- stretching (nas and nsym) at 1562 and 1418 cm-1. The latter showed a change in surface charge, in that the isoelectric point (IEP) changed from pH 3–4.5 to 8.5 when the MSN was functionalized with the amino groups, while carboxy-MSN showed a more negative charge in the whole pH range with respect to MSN. The hydrophilic character of the prepared materials was ascertained by quantitative microgravimetric measurements, allowing the calculation of the average isosteric adsorption heat (qst). This was found to be 51 +- 3 kJmol-1, 61+- 4, and 65 +- 3 kJmol-1 for MSN, amino- MSN, and carboxy-MSN samples, respectively. The increase in qst after functionalization can be ascribed to the specific interaction of water molecules with the functionalizing agents, in agreement with a higher basicity with respect to silanol groups. Moreover, the possibility of multiple H-bonding interactions of water molecules with the carboxylate anion is put forward to account for the higher water uptake with respect to parent MSN.File | Dimensione | Formato | |
---|---|---|---|
Musso PCCP OA.pdf
Open Access dal 23/04/2016
Descrizione: Articolo principale
Tipo di file:
POSTPRINT (VERSIONE FINALE DELL’AUTORE)
Dimensione
1.57 MB
Formato
Adobe PDF
|
1.57 MB | Adobe PDF | Visualizza/Apri |
Musso PCCP 15.pdf
Accesso riservato
Tipo di file:
PDF EDITORIALE
Dimensione
2.55 MB
Formato
Adobe PDF
|
2.55 MB | Adobe PDF | Visualizza/Apri Richiedi una copia |
I documenti in IRIS sono protetti da copyright e tutti i diritti sono riservati, salvo diversa indicazione.