This study evaluated the effectiveness of chemical-based adhesive techniques on promoting immediate and aged bond strength between zirconia and luting cement. A total of 128 discs of zirconia were divided into 4 groups (n = 32) according to the adhesive treatment: tribochemical silica-coating followed by silane (Silane Primer, Kerr) and bonding (Optibond FL, Kerr), Signum Zirconia Bond (Hereaus), Z-Prime Plus (Bisco), and All-Bond Universal (Bisco). Composite cylinders were cemented on the zirconia sample with Duo-Link Universal (Bisco). Eight specimens per group were subjected to 10,000 thermocycles and subsequently bond strength was tested with shear-bond strength test. ANOVA test showed that artificial aging significantly affected the bond strength to zirconia. Bonferroni test highlighted a significant influence of adhesive treatment (Signum) on bond strength after thermocycling. It was concluded that 10-MDP-based bonding systems showed no improvement in initial bond strength compared with tribochemical treatment. All chemical bonding techniques tested in this study were influenced by thermocycling.

Do chemical-based bonding techniques affect the bond strength stability to cubic zirconia?

Comba A.;Baldi A.;Michelotto Tempesta R.;Carossa M.;Perrone L.;Scotti N.
2021-01-01

Abstract

This study evaluated the effectiveness of chemical-based adhesive techniques on promoting immediate and aged bond strength between zirconia and luting cement. A total of 128 discs of zirconia were divided into 4 groups (n = 32) according to the adhesive treatment: tribochemical silica-coating followed by silane (Silane Primer, Kerr) and bonding (Optibond FL, Kerr), Signum Zirconia Bond (Hereaus), Z-Prime Plus (Bisco), and All-Bond Universal (Bisco). Composite cylinders were cemented on the zirconia sample with Duo-Link Universal (Bisco). Eight specimens per group were subjected to 10,000 thermocycles and subsequently bond strength was tested with shear-bond strength test. ANOVA test showed that artificial aging significantly affected the bond strength to zirconia. Bonferroni test highlighted a significant influence of adhesive treatment (Signum) on bond strength after thermocycling. It was concluded that 10-MDP-based bonding systems showed no improvement in initial bond strength compared with tribochemical treatment. All chemical bonding techniques tested in this study were influenced by thermocycling.
2021
Inglese
Esperti anonimi
14
14
1
9
9
10-MDP; Cubic zirconia; Shear-bond strength; Thermocycling; Tribochemical adhesion
1 – prodotto con file in versione Open Access (allegherò il file al passo 6 - Carica)
262
10
Comba A.; Baldi A.; Michelotto Tempesta R.; Carossa M.; Perrone L.; Saratti C.M.; Rocca G.T.; Femiano R.; Femiano F.; Scotti N.
info:eu-repo/semantics/article
open
03-CONTRIBUTO IN RIVISTA::03A-Articolo su Rivista
File in questo prodotto:
File Dimensione Formato  
materials-14-03920.pdf

Accesso aperto

Tipo di file: PDF EDITORIALE
Dimensione 286.4 kB
Formato Adobe PDF
286.4 kB Adobe PDF Visualizza/Apri

I documenti in IRIS sono protetti da copyright e tutti i diritti sono riservati, salvo diversa indicazione.

Utilizza questo identificativo per citare o creare un link a questo documento: https://hdl.handle.net/2318/1849902
Citazioni
  • ???jsp.display-item.citation.pmc??? 5
  • Scopus 9
  • ???jsp.display-item.citation.isi??? 6
social impact