The present study aimed to evaluate the wear rate of polymer-infiltrated network composites and ceramics against enamel in a bruxism-simulated scenario. Ninety-six (n = 96) molars were divided into six groups (n = 16) according to their occlusal material: group 1-a polymer-infiltrated network ceramic (PINC); group 2-a second polymer-infiltrated network ceramic (PINC2); group 3-nanohybrid resin-based composite (CO); group 4-cubic zirconia (ZR); group 5-lithium disilicate (LS); and group 6-sound enamel (EN). A laser scanner was used to digitalize all of the occlusal surfaces before and after a fatigue test, which was conducted with a chewing simulator set at 80 N and semicircular movement in order to simulate bruxist movement and loads. Statistical analysis of volume loss was performed with a one-way ANOVA and post hoc Bonferroni test. ZR had significantly inferior wear to PINC (p <= 0.01) and CO (p = 0.04). LS wore the antagonist enamel significantly more than PINC, CO, PINC2 and EN (p <= 0.01). On the other hand, ZR wore the antagonist enamel significantly more than CO (p <= 0.01) and PINC2 (p = 0.05). In conclusion, PINCs better preserved antagonist enamel at the expense of a higher wear of their own. LS causes significantly higher enamel wear compared with PINCs. ZR caused significantly higher enamel wear compared with CO and PINC2, but it was wear-resistant.

Wear Behaviour of Polymer-Infiltrated Network Ceramics, Lithium Disilicate and Cubic Zirconia against Enamel in a Bruxism-Simulated Scenario

Baldi, Andrea
Co-first
;
Carossa, Massimo
Co-first
;
Comba, Allegra;Alovisi, Mario;Pasqualini, Damiano;Berutti, Elio;Scotti, Nicola
Last
2022-01-01

Abstract

The present study aimed to evaluate the wear rate of polymer-infiltrated network composites and ceramics against enamel in a bruxism-simulated scenario. Ninety-six (n = 96) molars were divided into six groups (n = 16) according to their occlusal material: group 1-a polymer-infiltrated network ceramic (PINC); group 2-a second polymer-infiltrated network ceramic (PINC2); group 3-nanohybrid resin-based composite (CO); group 4-cubic zirconia (ZR); group 5-lithium disilicate (LS); and group 6-sound enamel (EN). A laser scanner was used to digitalize all of the occlusal surfaces before and after a fatigue test, which was conducted with a chewing simulator set at 80 N and semicircular movement in order to simulate bruxist movement and loads. Statistical analysis of volume loss was performed with a one-way ANOVA and post hoc Bonferroni test. ZR had significantly inferior wear to PINC (p <= 0.01) and CO (p = 0.04). LS wore the antagonist enamel significantly more than PINC, CO, PINC2 and EN (p <= 0.01). On the other hand, ZR wore the antagonist enamel significantly more than CO (p <= 0.01) and PINC2 (p = 0.05). In conclusion, PINCs better preserved antagonist enamel at the expense of a higher wear of their own. LS causes significantly higher enamel wear compared with PINCs. ZR caused significantly higher enamel wear compared with CO and PINC2, but it was wear-resistant.
2022
10
1682
1
10
bruxism; polymer-infiltrated network ceramics; wear; zirconia
Baldi, Andrea; Carossa, Massimo; Comba, Allegra; Alovisi, Mario; Femiano, Felice; Pasqualini, Damiano; Berutti, Elio; Scotti, Nicola
File in questo prodotto:
File Dimensione Formato  
biomedicines-10-01682-v2.pdf

Accesso aperto

Tipo di file: PDF EDITORIALE
Dimensione 1.19 MB
Formato Adobe PDF
1.19 MB Adobe PDF Visualizza/Apri

I documenti in IRIS sono protetti da copyright e tutti i diritti sono riservati, salvo diversa indicazione.

Utilizza questo identificativo per citare o creare un link a questo documento: https://hdl.handle.net/2318/1880454
Citazioni
  • ???jsp.display-item.citation.pmc??? 4
  • Scopus 8
  • ???jsp.display-item.citation.isi??? 9
social impact