ITQ-1 layered zeolites, with MWW framework, were prepared using different synthesis and calcination procedures and fully characterized by means of X-ray diffraction, scanning electron microscopy, N2 sorption and vibrational and nuclear magnetic resonance spectroscopies. Exploring different compositions of the precursor gel, the role of the Organic Structure Directing Agent (OSDA) was definitely disclosed. We proved that the concentration of OSDA in the synthesis gel affects the short-range crystalline order of zeolite crystals. In particular, diluted precursor gels led to the formation of low-density materials in the form of hollow spheres, with partially disordered layers, thinner crystals and high defectivity. In general, all ITQ-1 samples had the same crystalline structure but different morphology, either rose-like or hollow spheres. Moreover, the calcination procedure had an impact on the structural defects of the ITQ-1 zeolite: the higher the removal rate of the OSDA, the higher the defectivity degree of the zeolite.
Insight on MWW siliceous zeolites: From 2D precursors toward 3D structure
Rosso, Francesca;Airi, Alessia;Signorile, Matteo;Bordiga, Silvia;Crocellà, Valentina;Bonino, Francesca
2024-01-01
Abstract
ITQ-1 layered zeolites, with MWW framework, were prepared using different synthesis and calcination procedures and fully characterized by means of X-ray diffraction, scanning electron microscopy, N2 sorption and vibrational and nuclear magnetic resonance spectroscopies. Exploring different compositions of the precursor gel, the role of the Organic Structure Directing Agent (OSDA) was definitely disclosed. We proved that the concentration of OSDA in the synthesis gel affects the short-range crystalline order of zeolite crystals. In particular, diluted precursor gels led to the formation of low-density materials in the form of hollow spheres, with partially disordered layers, thinner crystals and high defectivity. In general, all ITQ-1 samples had the same crystalline structure but different morphology, either rose-like or hollow spheres. Moreover, the calcination procedure had an impact on the structural defects of the ITQ-1 zeolite: the higher the removal rate of the OSDA, the higher the defectivity degree of the zeolite.File | Dimensione | Formato | |
---|---|---|---|
Rosso-et-al_MicroMeso_2024_ITQ-1.pdf
Accesso aperto
Descrizione: Manuscript
Tipo di file:
PDF EDITORIALE
Dimensione
9.51 MB
Formato
Adobe PDF
|
9.51 MB | Adobe PDF | Visualizza/Apri |
Rosso-et-al_MicroMeso_2024_ESI.docx
Accesso aperto
Descrizione: Supporting information
Tipo di file:
POSTPRINT (VERSIONE FINALE DELL’AUTORE)
Dimensione
15.89 MB
Formato
Microsoft Word XML
|
15.89 MB | Microsoft Word XML | Visualizza/Apri |
I documenti in IRIS sono protetti da copyright e tutti i diritti sono riservati, salvo diversa indicazione.