The underlying mechanism driving the structural amorphous-to-crystalline transition in Group VI chalcogenides is still a matter of debate even in the simplest GeTe system. We exploit the extreme sensitivity of 57Fe emission Mössbauer spectroscopy, following dilute implantation of 57Mn (T½ = 1.5 min) at ISOLDE/CERN, to study the electronic charge distribution in the immediate vicinity of the 57Fe probe substituting Ge (FeGe), and to interrogate the local environment of FeGe over the amorphous-crystalline phase transition in GeTe thin films. Our results show that the local structure of as-sputtered amorphous GeTe is a combination of tetrahedral and defect-octahedral sites. The main effect of the crystallization is the conversion from tetrahedral to defect-free octahedral sites. We discover that only the tetrahedral fraction in amorphous GeTe participates to the change of the FeGe-Te chemical bonds, with a net electronic charge density transfer of ~ 1.6 e/a0 between FeGe and neighboring Te atoms. This charge transfer accounts for a lowering of the covalent character during crystallization. The results are corroborated by theoretical calculations within the framework of density functional theory. The observed atomic-scale chemical-structural changes are directly connected to the macroscopic phase transition and resistivity switch of GeTe thin films.

Atomic-scale study of the amorphous-to-crystalline phase transition mechanism in GeTe thin films

Fanciulli M;
2017-01-01

Abstract

The underlying mechanism driving the structural amorphous-to-crystalline transition in Group VI chalcogenides is still a matter of debate even in the simplest GeTe system. We exploit the extreme sensitivity of 57Fe emission Mössbauer spectroscopy, following dilute implantation of 57Mn (T½ = 1.5 min) at ISOLDE/CERN, to study the electronic charge distribution in the immediate vicinity of the 57Fe probe substituting Ge (FeGe), and to interrogate the local environment of FeGe over the amorphous-crystalline phase transition in GeTe thin films. Our results show that the local structure of as-sputtered amorphous GeTe is a combination of tetrahedral and defect-octahedral sites. The main effect of the crystallization is the conversion from tetrahedral to defect-free octahedral sites. We discover that only the tetrahedral fraction in amorphous GeTe participates to the change of the FeGe-Te chemical bonds, with a net electronic charge density transfer of ~ 1.6 e/a0 between FeGe and neighboring Te atoms. This charge transfer accounts for a lowering of the covalent character during crystallization. The results are corroborated by theoretical calculations within the framework of density functional theory. The observed atomic-scale chemical-structural changes are directly connected to the macroscopic phase transition and resistivity switch of GeTe thin films.
2017
7
8234
1
12
Mantovan R; Fallica R; Gerami AM; Molholt TE; Wiemer C; Longo M; Gunnlaugsson HP; Johnston K; Masenda H; Naidoo D; Ncube M; Bharuth-Ram K; Fanciulli M...espandi
File in questo prodotto:
File Dimensione Formato  
s41598-017-08275-5.pdf

Accesso aperto

Tipo di file: PDF EDITORIALE
Dimensione 2.44 MB
Formato Adobe PDF
2.44 MB Adobe PDF Visualizza/Apri

I documenti in IRIS sono protetti da copyright e tutti i diritti sono riservati, salvo diversa indicazione.

Utilizza questo identificativo per citare o creare un link a questo documento: https://hdl.handle.net/2318/2079751
Citazioni
  • ???jsp.display-item.citation.pmc??? ND
  • Scopus ND
  • ???jsp.display-item.citation.isi??? 22
social impact