TGA, MS and DSC of a solid polymeric Ge hydride, obtained by γ-radiolysis of GeH4, are reported. Upon heating, it undergoes two successive weight losses at 463 and 1173 K. At 948 K two crystal phases are formed, one of them is pure germanium. Some comparisons with a-Ge: H produced via RF sputtering or glow discharge are reported.

Thermolysis and mass spectra of polymeric germanium hydride produced by -radiolysis

BENZI, Paola;CASTIGLIONI, Mario;VOLPE, Paolo Edoardo Angelo;BATTEZZATI, Livio;
1988-01-01

Abstract

TGA, MS and DSC of a solid polymeric Ge hydride, obtained by γ-radiolysis of GeH4, are reported. Upon heating, it undergoes two successive weight losses at 463 and 1173 K. At 948 K two crystal phases are formed, one of them is pure germanium. Some comparisons with a-Ge: H produced via RF sputtering or glow discharge are reported.
1988
7
597
600
Thermolysis; Radiolysis; Germanium Hydride
P.Benzi; M. Castiglioni; P. Volpe; L. Battezzati; M.Venturi
File in questo prodotto:
Non ci sono file associati a questo prodotto.

I documenti in IRIS sono protetti da copyright e tutti i diritti sono riservati, salvo diversa indicazione.

Utilizza questo identificativo per citare o creare un link a questo documento: https://hdl.handle.net/2318/115918
Citazioni
  • ???jsp.display-item.citation.pmc??? ND
  • Scopus 22
  • ???jsp.display-item.citation.isi??? 24
social impact