The photocatalytic decomposition of yperite (bis(2-chloroethyl) sulfide), a chemical warfare agent, was achieved by using titania-silica catalysts doped with several transition metal ions. The preparation of these catalysts was achieved by impregnation of a titania-silica mixed oxide previously synthesized using a sol-gel route with salts of the doping elements (vanadium, iron, manganese). The above catalysts were characterized using several spectroscopic techniques: FTIR, Raman, DR-UV-Vis, and XPS. The band gap energy was measured for each photocatalytic system. The reaction was carried out in two different types of reactors, i.e. naturally aerated and a closed quartz tube aerated under a constant flow, and using two types of irradiation, UV-Vis and Vis. The investigated systems proved to be extremely active, leading to an almost complete degradation of yperite in 2 h of irradiation. An excellent correlation between the photocatalytic performances and the band gap has been found. Based on the characterization data and on the temporal evolution of the reaction products, a reaction mechanism has been suggested. This mechanism considers two distinct pathways for the decomposition of yperite, namely the C-S bond cleavage and the S oxidation.

Photo-degradation of yperite over V, Fe and Mn-doped titania- silica photocatalysts

DAMIN, Alessandro Ali;BORDIGA, Silvia;ZECCHINA, Adriano
2008-01-01

Abstract

The photocatalytic decomposition of yperite (bis(2-chloroethyl) sulfide), a chemical warfare agent, was achieved by using titania-silica catalysts doped with several transition metal ions. The preparation of these catalysts was achieved by impregnation of a titania-silica mixed oxide previously synthesized using a sol-gel route with salts of the doping elements (vanadium, iron, manganese). The above catalysts were characterized using several spectroscopic techniques: FTIR, Raman, DR-UV-Vis, and XPS. The band gap energy was measured for each photocatalytic system. The reaction was carried out in two different types of reactors, i.e. naturally aerated and a closed quartz tube aerated under a constant flow, and using two types of irradiation, UV-Vis and Vis. The investigated systems proved to be extremely active, leading to an almost complete degradation of yperite in 2 h of irradiation. An excellent correlation between the photocatalytic performances and the band gap has been found. Based on the characterization data and on the temporal evolution of the reaction products, a reaction mechanism has been suggested. This mechanism considers two distinct pathways for the decomposition of yperite, namely the C-S bond cleavage and the S oxidation.
2008
10
6562
6570
http://www.rsc.org/publishing/journals/CP/article.asp?doi=b810200g
SOL-GEL METHOD; STRUCTURAL-CHARACTERIZATION; SULFIDES; OXIDATION; CATALYSTS; WATER; TIO2; DECONTAMINATION; PHOTOOXIDATION; FTIR; Raman; DR-UV-Vis; XPS
S. Neatu; V.I. Parvulescu; G. Epure; E. Preda; V. Somoghi; A. Damin; S. Bordiga; A. Zecchina
File in questo prodotto:
File Dimensione Formato  
PCCP_Yprite.pdf

Accesso riservato

Tipo di file: POSTPRINT (VERSIONE FINALE DELL’AUTORE)
Dimensione 877.43 kB
Formato Adobe PDF
877.43 kB Adobe PDF   Visualizza/Apri   Richiedi una copia

I documenti in IRIS sono protetti da copyright e tutti i diritti sono riservati, salvo diversa indicazione.

Utilizza questo identificativo per citare o creare un link a questo documento: https://hdl.handle.net/2318/59900
Citazioni
  • ???jsp.display-item.citation.pmc??? ND
  • Scopus 22
  • ???jsp.display-item.citation.isi??? 21
social impact